Specification:
1) Carcass: EP100~EP400, NN100~NN400, TN/C & CC
2) No.s of ply: 2~10
3) Constructure: Fabric carcass, steel mesh reinforcement layer, top & bottom rubber cover
4) Delivery Detail: 20~30 working day for general orders
Characteristics:
Belt body light and thin, high tensile strength, moisture resistant, fatigue resistant, impact resistant, excellent trough ability etc.
Classify by performance:
1) General use conveyor belt,
2) Oil-resistant conveyor belt,
3) Acid/alkali conveyor belt,
4) Cold-resistant conveyor belt,
5) Anti-static electricity conveyor belt, etc.
Application:
Widely used in coal mine and other fire or high-temperature occasions.
Specification |
SN400 |
SN630 |
SN800 |
SN1000 |
SN1125 |
Tensile Strength (N/mm) |
400 |
630 |
800 |
1000 |
1125 |
Metal Mesh Thickness (mm) |
5.5 |
5.5 |
7.0 |
8.0 |
9.0 |
Top Rubber Cover Thickness (mm) |
6 |
8 |
9 |
10 |
10 |
Bottom Rubber Cover Thickness (mm) |
3 |
3 |
3 |
3 |
3 |
Interlayer Adhesive Strength Longitudinal Average Value of the Samples |
Ordinary Temperuture |
≥10N/mm |
160ºC |
≥4.0N/mm |
Min. Pulley Diameter (mm) |
|
150 |
200 |
300 |
400 |
500 |
Belt Width (mm) |
|
300-800 |
Cover Layer Physical Properties After Thermal Aging Test |
Item |
Type |
Type1 |
Type2 |
Type3 |
Type4 |
Changing scope |
Hardness |
Differences of before and after aging test |
+20 |
±20 |
±20 |
±20 |
Max. after aging test |
85 |
85 |
85 |
85 |
Tensile strength |
Properties changing rate reducing |
-25 |
-30 |
-40 |
-40 |
Min. after aging test |
12 |
10 |
5 |
|
Elongation at breaking |
Changing rate of properties |
-50 |
-50 |
-55 |
-55 |
Min. after aging test |
200 |
200 |
180 |
180 |
Note: Aging test (100°Cx168h, 125°Cx168h, 150°Cx168h) |