Application :
The burning-through resistant conveyor belt can be widely used in metallurgical, casting,cement and chemical industries for conveying of materials whose temperature can reach 150-250
Feature:
The reinforcement ply of the belt used by the special glass-fibre,(called GF fabric ) .It is heat resistant is good . The conveyor belt has excellent stability and high -heat resistant ,so the belt service life is prolonged.
Type of Fabric |
Reinforcement D.S EP |
cover thickness(mm) |
No of ply |
width range (mm) |
GF |
EP |
Strength of Mono Ply N/mm |
top |
bottom |
GF |
DSEP |
|
GF |
D.SEP100 |
100 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP150 |
150 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP200 |
200 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP250 |
250 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP300 |
300 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP350 |
350 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
GF |
D.SEP400 |
400 |
>=7 |
>=3 |
1 |
2-6 |
450-2800 |
Cover Layer Physical Properties After Thermal Aging Test |
Item |
Type |
Type1 |
Type2 |
Type3 |
Type4 |
Changing scope |
Hardness |
Differences of before and after aging test |
+20 |
±20 |
±20 |
±20 |
Max. after aging test |
85 |
85 |
85 |
85 |
Tensile strength |
Properties changing rate reducing |
-25 |
-30 |
-40 |
-40 |
Min. after aging test |
12 |
10 |
5 |
|
Elongation at breaking |
Changing rate of properties |
-50 |
-50 |
-55 |
-55 |
Min. after aging test |
200 |
200 |
180 |
180 |
Note: Aging test (100°Cx168h, 125°Cx168h, 150°Cx168h) |