Customization: | Available |
---|---|
Type: | Conveyor Belt |
Feature: | Wear-resistant, Heat-resistant, Tear-resistant, Flame-resistant, Cold-resistant |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Cover Layer Physical Properties After Thermal Aging Test |
|||||
Item | Type | ||||
Type1 | Type2 | Type3 | Type4 | ||
Changing scope | |||||
Hardness | Differences of before and after aging test | +20 | ±20 | ±20 | ±20 |
Max. after aging test | 85 | 85 | 85 | 85 | |
Tensile strength | Properties changing rate reducing | -25 | -30 | -40 | -40 |
Min. after aging test | 12 | 10 | 5 | ||
Elongation at breaking | Changing rate of properties | -50 | -50 | -55 | -55 |
Min. after aging test | 200 | 200 | 180 | 180 | |
Note: Aging test (100°Cx168h, 125°Cx168h, 150°Cx168h) |